修補仿大理石電梯門套方式介紹
2016-05-04 18:04:21 文章來源:www.81577.com.cn
1常用方法是:用刷子配合清水沖洗或用高壓水沖刷(此方法板材不能懸空),刷子可以有效清除石材表面及縫隙內的粉塵,使樹脂與石材接觸面增加,但由于水會涌入石材縫隙內,水的存在阻礙樹脂更深進入石材孔隙內,板材清潔后需要風干或自然風干,但常規風干方法仍會有水份殘留在仿大理石電梯門套孔隙內。
One commonly used method is: with a brush with water flushing or with high-pressure water washing (the plate can not be left vacant), brush can effectively remove the stone surface and crevices of the dust, so as to increase the contact surface of the resin and the stone, but due to water influx in crevice of stone, the presence of water hinder resin deeper into the stone pore, clean sheet need air dry or dry naturally. However, the conventional drying method will still have water remain in the imitation marble elevator door pore.
如需水份寒舍析出,采用隧道式或塔式兩種烘干設備進行烘干,測試控制在45度~55度,時間在120分鐘左右,但不同材質采用不同的時間控制,材質越疏松烘干時間越短,縫隙內水份完全烘干后,如有條件可以邊補膠邊真空器吸出縫隙的空氣,這樣樹脂就可以更深入進入縫隙,效果更好。
For my humble home water precipitation, the tunnel type or tower two drying equipment for drying test control at 45 degrees to 55 degrees, time 120 minutes, but of different materials by different time control, material more loose the drying time is short, gap, full of water after drying, such as conditions can edge patch edge rubber vacuum aspirator gap of air. This resin can deeper into the slot, the effect is better.
2鋪環氧樹脂,固化拋光處理
Shop 2, epoxy resin, curing polishing
環氧樹脂經加熱融化后倒在仿大理石電梯門套表面通常采用人工均勻涂抹在石材表面,涂抹百度在0.50mm到1mm,抹平過程中要施加一定的壓力使樹脂進入縫隙內。
Epoxy resin after being heated and melted down in imitation marble elevator door surface usually uses artificial evenly coated on the surface of the stone, smear Baidu in 0.50 mm to 1 mm, smooth process to a certain pressure is applied in the resin into the gap.
如大平采用自動化機械層,仿大理石電梯門套平鋪樹脂后送入烘干容器內,容器間諜控制在30~40度,時間約為120分鐘,由電腦控制,不能震動,如在常溫下需靜止放置 24小時左右,樹脂才能完全固化,待樹脂與材質融合為一體后,此補膠過程全部完全,通過補膠后的仿大理石電梯門套經磨拋后機械強度提高、色澤更均勻、艷麗。
Such as flat by mechanical automation layer, imitation marble elevator door tile resin into the drying container, the container spy control in 30 ~ 40 degrees, about 120 minutes, controlled by a computer, that cannot be shaken, such as at room temperature required to be still placed for about 24 hours, the resin can finish all solid state, until the resin and the combination of materials for one, the glue filling process altogether by glue after repair of imitation marble elevator door by grinding and polishing mechanical strength increased, the color more uniform, gorgeous.
One commonly used method is: with a brush with water flushing or with high-pressure water washing (the plate can not be left vacant), brush can effectively remove the stone surface and crevices of the dust, so as to increase the contact surface of the resin and the stone, but due to water influx in crevice of stone, the presence of water hinder resin deeper into the stone pore, clean sheet need air dry or dry naturally. However, the conventional drying method will still have water remain in the imitation marble elevator door pore.
如需水份寒舍析出,采用隧道式或塔式兩種烘干設備進行烘干,測試控制在45度~55度,時間在120分鐘左右,但不同材質采用不同的時間控制,材質越疏松烘干時間越短,縫隙內水份完全烘干后,如有條件可以邊補膠邊真空器吸出縫隙的空氣,這樣樹脂就可以更深入進入縫隙,效果更好。
For my humble home water precipitation, the tunnel type or tower two drying equipment for drying test control at 45 degrees to 55 degrees, time 120 minutes, but of different materials by different time control, material more loose the drying time is short, gap, full of water after drying, such as conditions can edge patch edge rubber vacuum aspirator gap of air. This resin can deeper into the slot, the effect is better.
2鋪環氧樹脂,固化拋光處理
Shop 2, epoxy resin, curing polishing
環氧樹脂經加熱融化后倒在仿大理石電梯門套表面通常采用人工均勻涂抹在石材表面,涂抹百度在0.50mm到1mm,抹平過程中要施加一定的壓力使樹脂進入縫隙內。
Epoxy resin after being heated and melted down in imitation marble elevator door surface usually uses artificial evenly coated on the surface of the stone, smear Baidu in 0.50 mm to 1 mm, smooth process to a certain pressure is applied in the resin into the gap.
如大平采用自動化機械層,仿大理石電梯門套平鋪樹脂后送入烘干容器內,容器間諜控制在30~40度,時間約為120分鐘,由電腦控制,不能震動,如在常溫下需靜止放置 24小時左右,樹脂才能完全固化,待樹脂與材質融合為一體后,此補膠過程全部完全,通過補膠后的仿大理石電梯門套經磨拋后機械強度提高、色澤更均勻、艷麗。
Such as flat by mechanical automation layer, imitation marble elevator door tile resin into the drying container, the container spy control in 30 ~ 40 degrees, about 120 minutes, controlled by a computer, that cannot be shaken, such as at room temperature required to be still placed for about 24 hours, the resin can finish all solid state, until the resin and the combination of materials for one, the glue filling process altogether by glue after repair of imitation marble elevator door by grinding and polishing mechanical strength increased, the color more uniform, gorgeous.